SAA7113H NXP Semiconductors, SAA7113H Datasheet - Page 71

SAA7113H

Manufacturer Part Number
SAA7113H
Description
Manufacturer
NXP Semiconductors
Datasheet

Specifications of SAA7113H

Video Resolution (max)
720Pixels
Pin Count
44
Package Type
PQFP
Lead Free Status / RoHS Status
Compliant

Available stocks

Company
Part Number
Manufacturer
Quantity
Price
Part Number:
SAA7113H
Manufacturer:
NXP
Quantity:
55
Part Number:
SAA7113H
Manufacturer:
NXP
Quantity:
2 428
Part Number:
SAA7113H
Manufacturer:
PHI
Quantity:
1 000
Part Number:
SAA7113H
Manufacturer:
PHILIPS
Quantity:
20 000
Company:
Part Number:
SAA7113H
Quantity:
51
Part Number:
SAA7113H/V2
Manufacturer:
NXP
Quantity:
12 000
Part Number:
SAA7113H/V2
Manufacturer:
PHI/PBF
Quantity:
3
Part Number:
SAA7113H/V2
Manufacturer:
PHILIPS
Quantity:
8
Part Number:
SAA7113H/V2
Manufacturer:
NXP/恩智浦
Quantity:
20 000
Company:
Part Number:
SAA7113H/V2
Quantity:
204
Part Number:
SAA7113H/V2,518
Manufacturer:
Sigma Designs Inc
Quantity:
10 000
Philips Semiconductors
9397 750 14232
Product data sheet
18.4 Manual soldering
18.5 Package related soldering information
During placement and before soldering, the package must be fixed with a droplet of
adhesive. The adhesive can be applied by screen printing, pin transfer or syringe
dispensing. The package can be soldered after the adhesive is cured.
Typical dwell time of the leads in the wave ranges from 3 seconds to 4 seconds at 250 C
or 265 C, depending on solder material applied, SnPb or Pb-free respectively.
A mildly-activated flux will eliminate the need for removal of corrosive residues in most
applications.
Fix the component by first soldering two diagonally-opposite end leads. Use a low voltage
(24 V or less) soldering iron applied to the flat part of the lead. Contact time must be
limited to 10 seconds at up to 300 C.
When using a dedicated tool, all other leads can be soldered in one operation within
2 seconds to 5 seconds between 270 C and 320 C.
Table 81:
[1]
[2]
[3]
Package
BGA, HTSSON..T
SSOP..T
DHVQFN, HBCC, HBGA, HLQFP, HSO, HSOP,
HSQFP, HSSON, HTQFP, HTSSOP, HVQFN,
HVSON, SMS
PLCC
LQFP, QFP, TQFP
SSOP, TSSOP, VSO, VSSOP
CWQCCN..L
– smaller than 1.27 mm, the footprint longitudinal axis must be parallel to the
The footprint must incorporate solder thieves at the downstream end.
For packages with leads on four sides, the footprint must be placed at a 45 angle to
the transport direction of the printed-circuit board. The footprint must incorporate
solder thieves downstream and at the side corners.
For more detailed information on the BGA packages refer to the (LF)BGA Application Note (AN01026);
order a copy from your Philips Semiconductors sales office.
All surface mount (SMD) packages are moisture sensitive. Depending upon the moisture content, the
maximum temperature (with respect to time) and body size of the package, there is a risk that internal or
external package cracks may occur due to vaporization of the moisture in them (the so called popcorn
effect). For details, refer to the Drypack information in the Data Handbook IC26; Integrated Circuit
Packages; Section: Packing Methods .
These transparent plastic packages are extremely sensitive to reflow soldering conditions and must on no
account be processed through more than one soldering cycle or subjected to infrared reflow soldering with
peak temperature exceeding 217 C
body peak temperature must be kept as low as possible.
[5]
transport direction of the printed-circuit board.
, SO, SOJ
[3]
[1]
, TFBGA, VFBGA, XSON
Suitability of surface mount IC packages for wave and reflow soldering methods
[8]
, PMFP
[3]
, LBGA, LFBGA, SQFP,
[9]
, WQCCN..L
Rev. 02 — 9 May 2005
[8]
10 C measured in the atmosphere of the reflow oven. The package
Soldering method
Wave
not suitable
not suitable
suitable
not recommended
not recommended
not suitable
[4]
© Koninklijke Philips Electronics N.V. 2005. All rights reserved.
9-bit video input processor
[5] [6]
[7]
SAA7113H
Reflow
suitable
suitable
suitable
suitable
suitable
not suitable
[2]
71 of 75

Related parts for SAA7113H